Product Details:

Place of Origin: China
Brand Name: OEM
Certification: ISO
Model Number: ASTM B348 GRADE I/II

Payment & Shipping Terms:

Minimum Order Quantity: 500 meters
Price: negotiable
Packaging Details: Linear anode On steel wheel
Delivery Time: 1FCL: 10 days
Payment Terms: L/C, D/P, T/T, Western Union, MoneyGram,Paypal
Supply Ability: 50000meters/month
Get Best Price Contact Now

Detail Information

Material: MMO Ti MIXED METAL OXIDE LINEAR ANODES Standard: ASTM B348
Content: Anode Linear MMO (Flex) Which Has Coke Anode Wire: 1mm
High Light:

sacrificial anode protection

,

mg anode

Product Description

MMO Ti MIXED METAL OXIDE LINEAR ANODE WITH COKE ANPDE WIRE 1MM

Activation: Noble Mixed Metal Oxides consisting of IrO2 and Ta2O5 Substrate Material: Titanium to ASTM Grade 1 or 2 Working Environment: Evolution of O2, Cl2 or a combination of both Nominal Design Life: Typically 20 years when operating at an anode current density of 100 A/m2 coating loading can be adjusted for any combination of current output and design life.

Technical Parameters TB39-52
Anode Diameter 39±2mm
MMO/Ti Anode Wire Diameter ≥0.8mm
Anode Design Life ≥40years
Anode Consumption (Including Filling) ≤6mg/A.a
Output Current (Maximum) 1500mA/m
Coating Thickness of Metal Oxide ≥ 6g/m2
Resistivity of Mixed Metal Oxides 10-5Ω.cm
Contact Resistance of Anode and Cable Joint ≤1.0 mΩ
Anode Resistance ≤0.007Ω∕m
Content of Coke Breeze Filler ≥ 98%
Coke Breeze Resistance ≤0.55 Ω·cm
Fabric Jacket Tube Anticorrosion,permeable
Fabric Jacket Mesh Wearproof,anti environmental temperature variability
Anode Weight ≥1.3kg/m
Anode Length(Each Unit) 700m(or made to order)

 

The design of a flexible anode can be divided into the following four steps:

(1) First, determine the required protection current. The protection current needs to be determined according to the condition of the protection layer of the protection pipeline. The density of the protection current can then be selected. The required current can be obtained by multiplying the protection area by the density of the current.

(2) The second is to design the loop, and to ensure that the designed flexible anode loop can ensure the current distribution throughout the length and ensure uniform distribution. The maximum loop length can be calculated from the confluence point to obtain the maximum length of the anode. . The subsequent current feed point is calculated based on the maximum length of the loop.

(3) Select the appropriate power supply equipment specifications, flexible anode also has its special place, its special place is that the resistance between cathode and anode is very low, taking into account the long conductor, we must use non-standard calculation.

(4) The last step is to select the accessories. When selecting the accessories of the flexible anode, the connection method should be used as the basis. The best filler material for flexible anodes is coke powder. When selecting coke powder, the carbon content should be more than 85% and particle size less than 3mm.

Mmo Ti Mixed Metal Oxide Anode Linear Mmo Flex With Coke Anode Wire 1mm 0

 

Other anode

 

* Zinc anodes (ASTM B418-95 US MILL 18001K)

* Al-Zn-In anodes (GAIII)

* Magnesium anodes ( ASTM-G97)

* High silicon cast iron anodes ( ASTM-A518-3,BS1591)

 

email: lucky@hbnewmaterial.com

Want to Know more details about this product
I am interested in Mmo Ti Mixed Metal Oxide Anode Linear Mmo Flex With Coke Anode Wire 1mm could you send me more details such as type, size, quantity, material, etc.
Thanks!
Waiting for your reply.