CuCr10 Copper Chromium Master Alloy For The Copper And Brass Industry
Product Details:
Place of Origin: | China |
Brand Name: | High Broad |
Certification: | ISO |
Model Number: | Copper-Chromium (CuCr) |
Payment & Shipping Terms:
Minimum Order Quantity: | 10 kgs |
---|---|
Price: | TBA |
Packaging Details: | CuCr in drum then on pallet for export |
Delivery Time: | 1000kgs: 1 days |
Payment Terms: | L/C, D/A, D/P, T/T, Western Union, MoneyGram,PayPal,West Union |
Supply Ability: | 100mt/month |
Detail Information |
|||
Material: | Copper-Chromium (CuCr) | Usage: | For The Copper And Brass Industry |
---|---|---|---|
1: | CuCr10 | 2: | CuCr20 |
High Light: | CuCr10 Copper Chromium Master Alloy,ISO Copper Chromium Master Alloy |
Product Description
CuCr10 Copper Chromium Master Alloy For The Copper And Brass Industry
These alloys have one thing in common: they dissolve better than the corresponding pure metal or metals.
The range includes alloys such as Copper-Chromium,Copper-Iron, Copper-Manganese, Copper-Boron and Copper-Zirconium.
Alloy Composition
Alloy | Composition |
CuCr10 | 10% Cr balance Cu |
CuCr20 | 20% Cr balance Cu |
The application of copper-based master alloys is precipitation hardening of alloyed copper. Typical applications include resistance welding electrodes, seam welding wheels and electrical and thermal conductors requiring more strength than provided by unalloyed copper.
Other Copper based allloys
Alloy | Composition |
CuZr40 | 40% Zr balance Cu |
CuZr50 | 50% Zr balance Cu |
Product | Grade | Chemicals% | Application | Add volume | Melting point℃ | properties |
CuSi | CuSi16 | Si13.5~16.5 | Add Si,improve plasticity | N.A | 800 | fragile |
CuMn | CuMn22 | Mn20~25 | Refine grains,improve plasticity,Eliminate hot rolling cracks | 2~3‰ | 850~900 | tough |
CuNi | CuNi15 | Ni14~18 | Add Ni, improve plasticity | 2~3‰ | 1050~1200 | tough |
CuFe | CuFe10 | Fe9~11 | Refine grains,Improve cold working plasticity | 3~5‰ | 1300~1400 | tough |
CuSb | CuSb50 | Sb49~51 | Refine grains | 2~3‰ | 680 | fragile |
CuBe | CuBe4 | Be3.8~4.8 | Refine grains | 1~3‰ | 1100~1200 | tough |
CuP | CuP14 | P13~15 | Refine grains,Deaeration and deoxygenation | 1~3‰ | 900~1020 | fragile |
CuMg | CuMg10 | Mg9~11 | Refine grains | 1~3‰ | 750~800 | fragile |
CuRe | CuRE15 | RE14~16 | Refine grains,Desulfurization,Deoxidation, improve performance, improve conductivity | 2~4‰ | 1050~1200 | tough |
CuTi | CuTi20 | Ti18~20 | Refine grains | 1~5‰ | 970~1020 | tough |
CuZr | CuZr10 | Zr8~12 | Refine grains | 2~3‰ | 1100~1200 | tough |
CuB | CuB3 | B3~3.8 | improve conductivity | 0.5~2‰ | 1200~1250 | tough |
Shape: ingot
Feel free contact with us for more detail by email: lucky@hbnewmaterial.com