• AlNb60 Niobium Aluminum Master Alloy Lumps 10-50mm Standard Grade for Nickel Superalloy Melting
  • AlNb60 Niobium Aluminum Master Alloy Lumps 10-50mm Standard Grade for Nickel Superalloy Melting
  • AlNb60 Niobium Aluminum Master Alloy Lumps 10-50mm Standard Grade for Nickel Superalloy Melting
AlNb60 Niobium Aluminum Master Alloy Lumps 10-50mm Standard Grade for Nickel Superalloy Melting

AlNb60 Niobium Aluminum Master Alloy Lumps 10-50mm Standard Grade for Nickel Superalloy Melting

Product Details:

Place of Origin: Hunan, China
Brand Name: HIGH BROAD
Certification: ISO 9001:2015
Model Number: AlNb60-LP-1050-STD

Payment & Shipping Terms:

Minimum Order Quantity: 25 kg
Price: USD 28-38 / kg
Packaging Details: 25 kg iron drum with moisture-proof aluminum foil vacuum inner bag, or 1000 kg ton bag
Delivery Time: 7-15 working days after order confirmation
Payment Terms: T/T, L/C
Supply Ability: 200 Metric Tons per Month
Get Best Price Contact Now

Detail Information

Product Name: AlNb60 Niobium Aluminum Master Alloy Form: Lumps
Particle Size: 10-50mm Nb Content: 55.0-65.0 Wt% (nominal 60%)
Al Content: Balance Fe Max: 0.20 Wt%
Si Max: 0.10 Wt% C Max: 0.08 Wt%
O Content: Controlled, Standard Grade Grade: Standard Grade
Standard: AMS / EN1676 Internal Control Application: Nickel Superalloy Melting
Highlight:

AlNb60 niobium aluminum master alloy lumps

,

10-50mm AlNb60 master alloy for melting

,

Standard grade niobium aluminum alloy

Product Description

AlNb60 Niobium Aluminum Master Alloy — Lumps 10-50mm

HIGH BROAD AlNb60 is a vacuum-grade niobium–aluminum master alloy with a nominal 60% Nb content (Nb 55–65 wt%, Al balance), supplied as lumps in 10-50mm. It is engineered for nickel-based superalloy melting, delivering a stable niobium recovery rate, excellent dissolution and wetting, and low segregation for consistent, repeatable melts.

Chemical Composition (wt%)

ElementSpecification
Nb55.0–65.0% (nominal 60%)
AlBalance
Fe≤ 0.20%
Si≤ 0.10%
C≤ 0.08%
OControlled, standard grade

Product Features

  • Stable niobium recovery rate with excellent dissolution and wetting behavior; pure Nb is refractory, while AlNb60 greatly lowers the addition difficulty.
  • β-phase stabilizing element that refines grain structure and improves high-temperature strength, creep resistance, corrosion resistance and thermal stability.
  • Low segregation, uniform composition and strong batch-to-batch consistency, suitable for continuous and vacuum melting.
  • Stable Nb Recovery Rate: standard, ideal for high-end and demanding melt shops.

Core Applications

  • Gamma-prime strengthened nickel-based superalloys
  • Improved high-temperature creep resistance
  • Turbine blades and hot-section components

Packaging & Delivery

  • Packaging: moisture-proof anti-rust aluminum foil vacuum bag / iron drum with inner moisture-proof bag, 25 kg per drum or 1000 kg ton bag.
  • Trade terms: FCA, FOB, DAP; exportable to the EU and Russia.
  • MOQ 25 kg, with larger tonnage scheduling and expedited trial orders available.

Quality Assurance

Each batch can be supplied with a Certificate of Analysis (COA), spectral test report and MSDS. Production is carried out to internal AMS / EN1676 control standards, and a high-purity controlled-impurity version is available on request.