10-50mm Granules AlNb60 Niobium Aluminum Master Alloy for Nickel Superalloy Melting with Stable Nb Recovery Rate
Product Details:
| Place of Origin: | Hunan, China |
| Brand Name: | HIGH BROAD |
| Certification: | ISO 9001:2015 |
| Model Number: | AlNb60-GR-1050-STD |
Payment & Shipping Terms:
| Minimum Order Quantity: | 25 kg |
|---|---|
| Price: | USD 28-38 / kg |
| Packaging Details: | 25 kg iron drum with moisture-proof aluminum foil vacuum inner bag, or 1000 kg ton bag |
| Delivery Time: | 7-15 working days after order confirmation |
| Payment Terms: | T/T,L/C |
| Supply Ability: | 200 Metric Tons per Month |
|
Detail Information |
|||
| Nb Content: | 55.0-65.0 Wt% (nominal 60%) | Particle Size: | 10-50mm |
|---|---|---|---|
| Fe Max: | 0.20 Wt% | Si Max: | 0.10 Wt% |
| C Max: | 0.08 Wt% | Al Content: | Balance |
| Highlight: | AlNb60 Niobium Master Alloy Granules,Nickel Superalloy Melting Additive,Stable Nb Recovery Rate |
||
Product Description
HIGH BROAD AlNb60 is a vacuum-grade niobium-aluminum master alloy with a nominal 60% Nb content (Nb 55–65 wt%, Al balance), supplied as granules in 10–50 mm. It is engineered for nickel-based superalloy melting, delivering a stable niobium recovery rate, excellent dissolution and wetting, and low segregation for consistent, repeatable melts.
| Element | Specification |
|---|---|
| Nb | 55.0–65.0% (nominal 60%) |
| Al | Balance |
| Fe | ≤ 0.20% |
| Si | ≤ 0.10% |
| C | ≤ 0.08% |
| O | Controlled, standard grade |
- Stable niobium recovery rate with excellent dissolution and wetting behavior; pure Nb is refractory, while AlNb60 greatly lowers the addition difficulty.
- β-phase stabilizing element that refines grain structure and improves high-temperature strength, creep resistance, corrosion resistance and thermal stability.
- Low segregation, uniform composition and strong batch-to-batch consistency, suitable for continuous and vacuum melting.
- Stable Nb recovery rate: standard grade, ideal for high-end and demanding melt shops.
- Gamma-prime strengthened nickel-based superalloys
- Improved high-temperature creep resistance
- Turbine blades and hot-section components
- Packaging: moisture-proof anti-rust aluminum foil vacuum bag / iron drum with inner moisture-proof bag, 25 kg per drum or 1000 kg ton bag.
- Trade terms: FCA, FOB, DAP; exportable to the EU and Russia.
- MOQ: 25 kg, with larger tonnage scheduling and expedited trial orders available.
Each batch can be supplied with a Certificate of Analysis (COA), spectral test report and MSDS. Production is carried out to internal AMS / EN1676 control standards, and a high-purity controlled-impurity version is available on request.